Wet tumble with a warm water, stainless steel media, couple drops of dawn platinum, and a teaspoon of citric acid polish (lemishine or whatever) and then just tumble for 90 minutes has been my process.
Separate with a spin separator then use a cheapo magnet from HF to put the steel back in my tumbler.
Separate with a spin separator then use a cheapo magnet from HF to put the steel back in my tumbler.