How often y'all anneal cases after firing? I have had some converted .308 to .243 cases crack at the mouth. I have had .45-70 brass crack after loading for about 5 times or so. I have started to anneal my .243 (bolt gun) and .308 (AR10) after every firing just to make things more consistent and less likely to crack from stress. My .223/5.56 brass ill probably anneal about 3 to 5 firings based on my batches of brass I recycle. It's a lot of work as I use double cotton glove and torch the cases by hand. Its not the best, but I figured it's alright.